Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKONITE® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated

Category Metal , Metal Matrix Composite , Nonferrous Metal , Molybdenum Alloy , Precious Metal , Silver Alloy , Refractory Metal
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.22 g/cc
0.3692 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 82
82
Flexural Modulus 0.931 GPa
135 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 250 W/m-K
1740 BTU-in/hr-ft²-°F
Melting Point 980 - 2610 °C
1800 - 4730 °F
Solidus 980 °C
1800 °F
Liquidus 2610 °C
4730 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 60 %
60 %
Silver, Ag 40 %
40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000383 ohm-cm
0.00000383 ohm-cm
(45% IACS)