Material Notes:
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Typical Physical and Chemical Characteristics: Filco 650 is an unsaturated modified polyester polymer in a non ionic water emulsion.Characteristics of the dried film: clearnon tackycompatible with unsaturated polyester and other thermosetslow soluble in styreneApplications: Filco 650 is suggested as a binder for performs and c.s. mat with low solubility in styrene. The use of organic peroxide as a source of free radicals is suggested. Benzoyl peroxide in water dispersion can for example be used at a level of 0.5 - 1.0% on Filco 650. Filco 650 is also suggested as a film former for glass fiber sizes for:roving for smcbmcInformation provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Solids Content 50 - 54 %
50 - 54 %
MA145LFE
Particle Size 1.0 - 2.5 µm
1.0 - 2.5 µm
MA147LFE
pH 1.5 - 3.5
1.5 - 3.5
MA148LFE
Viscosity 500 - 2500 cP

@Temperature 25.0 °C
500 - 2500 cP

@Temperature 77.0 °F
spindle n 3-10 RPM; MA143LFE
Descriptive Properties Value Comments
Appearance Milky Liquid