CTC X-PRO CTC PP1050 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer CTC (Composite Technologies)
Trade Name X-PRO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CTC X-PRO CTC PP1050 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
X-PRO PP 1050 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled compounds.Data provided by Composite Technologies (CTC).
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM-D792
Melt Flow 53 g/10 min
53 g/10 min
ASTM-D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
2 in/min; ASTM-D638
Elongation at Yield 10 %
10 %
2 in/min; ASTM-D638
Flexural Modulus, 1% Secant 1210 MPa
175000 psi
0.05 in/min; ASTM-D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM-D3418
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM-D648
Descriptive Properties Value Comments
Color General Purpose Black