Carmel Olefins IPETHENE® 470 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer Carmel Olefins
Trade Name IPETHENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins IPETHENE® 470 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IPETHENE® 470 is a low density polyethylene extrusion coating and lamination grade. This grade can be processed at high coating temperatures and coating speeds. It exhibits low neck-in and stable web edge, good adhesion to many substrates, excellent heat sealing properties, and low gel level. APPLICATIONS IPETHENE® 470 is used for extrusion coating of various materials, injection and blow molding articles, and compounds and masterbatches production.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183-A
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.5 MPa
1520 psi
ISO 527-2
Tensile Strength, Yield 10.5 MPa
1520 psi
ISO 527-2
Elongation at Break 500 %
500 %
ISO 527-2
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C

@Load 1.02 kg
198 °F

@Load 2.25 lb
ISO 306