Mechanical Properties Metric English Comments
Tenacity 0.412 - 0.500 N/tex
4.67 - 5.66 g/denier
EMS-Griltech Grilon® BS 22R Nylon 6 Monofilament (Super-Set)
Description: GRILON BS 22R is a Nylon 6 based monofilament for paper machine, clothing, forming screen, and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided ..
Tenacity 0.300 - 0.500 N/tex
3.40 - 5.66 g/denier
Cathay Terryl® Renewable Engineering Polyamide
Terryl® provides significant advantages in spinnability, dyeability, water absorption and comfort.Information provided by Cathay