Material Notes:
Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.26 g/cc
0.118 lb/in³
Weibull Modulus 10
10
Mechanical Properties Metric English Comments
Vickers Microhardness 1100
1100
Modulus of Elasticity 320 GPa
46400 ksi
Flexural Strength 330 MPa

@Temperature 23.0 °C
47900 psi

@Temperature 73.4 °F
Poissons Ratio 0.22
0.22
Fracture Toughness 2.50 MPa-m½
2.28 ksi-in½
Shear Modulus 131 GPa
19000 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 4.90 µm/m-°C

@Temperature 20.0 - 1000 °C
2.72 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 8.9
8.9
Descriptive Properties Value Comments
Grain Size, microns 4
Purity, % 99.8
Users viewing this material also viewed the following: