Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 555 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 80.0 - 100 W/m-K
555 - 694 BTU-in/hr-ft²-°F
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â..
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
Perpendicular (002)
Mateck Highly Oriented Pyrolytic Graphite
Oxidic single crystals. Applications include:Scanning tunneling microscopy-callibration and substratesGraphite monochromatorsx-ray diffractionneutron scattering and diffraction
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite
Cast, reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Thermal Conductivity >= 80.0 W/m-K
>= 555 BTU-in/hr-ft²-°F
H.C. Starck HPM 1800 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Thermal Conductivity >= 80.0 W/m-K
>= 555 BTU-in/hr-ft²-°F
H.C. Starck HPM 1810 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Thermal Conductivity >= 80.0 W/m-K
>= 555 BTU-in/hr-ft²-°F
H.C. Starck HPM 1850W Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek Hot Pressed Aluminum Nitride
Aluminum Nitride Advantages: High heat dissipation with thermal conductivity of 170 W/m K Non-toxic alternative to BeO Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors H..
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 1370-1E Aluminum Nitride
Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company