Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
PolyOne OnForce™ LFT NN-50LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 330 MPa | 47900 psi | |
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Flexural Strength | 330 MPa | 47900 psi | |
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Flexural Strength | 330 MPa | 47900 psi | |
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 330 MPa | 47900 psi | |
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Solvay Specialty Polymers Kalix® 2955 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2955 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where .. |
|||
Flexural Strength | 330 MPa | 47900 psi | GB/T 9341-2008 |
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 (Asia Pacific) LNP* Thermocomp* RF009S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 330 MPa | 47900 psi | DIN EN 843-1 |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |
|||
Flexural Strength | 330 MPa | 47900 psi | DIN EN 843-1 |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ASTM D790 |
Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned Ultra high-rigidityInformation provided by Unitika Ltd. |
|||
Flexural Strength | 330 MPa | 47900 psi | ASTM D790 |
Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber Heat stabilized, 50% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 330 MPa | 47900 psi | ASTM D790 |
Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber 50% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 330 MPa @Temperature 23.0 °C |
47900 psi @Temperature 73.4 °F |
|
Ceradyne Ceralloy® 1370-1E Aluminum Nitride Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Flexural Strength | 330 MPa | 47900 psi | DIN EN 843-1 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |
|||
Flexural Strength | 330 MPa | 47900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of .. |
|||
Flexural Strength | 330 MPa | 47900 psi | ISO 178 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 330 MPa | 47900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 (Asia Pacific) LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Asia Pacific region. |