Material Notes:
Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft sealsLightweight generators, usually for aircraftVane actuators for missiles Particle beam focusing, quadrupoles, lenses, wigglers, etc.Magnetic bearings, gyros, vacuum pumps, accelerometers Various mechanisms in disk drives, cameras, tape drives, and miniature loudspeakers and earphones; where small size is important Information provided by Ceradyne Company
Physical Properties Metric English Comments
Density 8.40 g/cc
0.303 lb/in³
Thermal Properties Metric English Comments
Thermal Conductivity 10.5 W/m-K
72.5 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000500 ohm-cm
0.0000500 ohm-cm
Magnetic Coercive Force, Hc >= 1800 Oe
>= 1800 Oe
Intrinsic
5600 - 7000 Oe
5600 - 7000 Oe
Magnetic Remanence, Br 5800 - 7200 Gauss
5800 - 7200 Gauss
Magnetic Maximum Energy Product, BH 9.0 - 13 MGOe
9.0 - 13 MGOe
Curie Temperature 700 °C
1290 °F
Descriptive Properties Value Comments
Room Temperature Compensation, RTC, %/°C 0/-0.03