Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | In-Plane |
GrafTech eGRAF® SPREADERSHIELD™ SS1500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Momentive Performance Materials Zirconium Carbide (ZrC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Electrical Resistivity | 0.0000500 - 0.0000600 ohm-cm | 0.0000500 - 0.0000600 ohm-cm | |
Alliance S-20A Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000500 - 0.0000600 ohm-cm | 0.0000500 - 0.0000600 ohm-cm | |
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000500 - 0.0000600 ohm-cm | 0.0000500 - 0.0000600 ohm-cm | |
Alliance S-26A Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Ceradyne SEMICORE® S1-5C Specials SmCo5 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Ceradyne SEMICORE® S2-17B MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Ceradyne SEMICORE® S2-17C Specials Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000 The alloy produces good magnetic properties, wide latitude to control hysteresis loop shape via recrystallization modes. Applications for this grade range from electromechanical relay cores, to ver.. |
|||
Electrical Resistivity | 0.0000500 - 0.0000600 ohm-cm | 0.0000500 - 0.0000600 ohm-cm | |
Alliance S-22A Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000500 ohm-cm | 0.0000500 ohm-cm | |
Ceradyne SEMICORE® S2-17A MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
Electrical Resistivity | 0.0000500 - 0.0000600 ohm-cm | 0.0000500 - 0.0000600 ohm-cm | |
Alliance S-22B Samarium Cobalt Magnetic Material |