Material Notes:
Features: High heat resistanceForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 3.5 g/10 min
3.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 43.0 MPa
6230 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 61.4 MPa
8900 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 2.30 J/cm
4.30 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: