Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Recycled contentForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.022 cm/cm
0.022 in/in
0.125 in; ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
0.125 in; ASTM D955
Melt Flow 10.5 g/10 min
10.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 79.3 MPa
11500 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) 113 °C
235 °F
Unannealed; ASTM D648