Chase Plastics CP Pryme® N140MGHSL (DAM) Nylon 6, 40% Mineral/Glass Reinforced, Heat Stabilized, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N140MGHSL (DAM) Nylon 6, 40% Mineral/Glass Reinforced, Heat Stabilized, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 124 MPa
18000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
395 °F
ASTM D648