Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.69 GPa | 245 ksi | Tangent; ASTM D790 |
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
PolyOne Stat-Tech™ PP-16CP/000-2 HI Polypropylene, Unspecified (PP, Unspecified) Stat-Tech™ electrically conductive compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic applications. These compounds combine .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Flexural Modulus | 1.69 - 8.27 GPa | 245 - 1200 ksi | Average value: 3.45 GPa Grade Count:43 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 1% Secant; ASTM D790A |
Ineos H44N-00 Polypropylene Homopolymer H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D 790 |
Styrolution PS 5410 HIPS Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100MD2 (COND, 50% RH) Nylon 66 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 5143H Homopolymer Polypropylene Hopolymer Formolene® 5143H is a polypropylene homopolymer designed for sheet and thermoforming applications requiring good clarity. It contains a unique combination of stabilizers, nucleators and a.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ BMV 201 Performance Polyolefin Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive e.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | Chord, 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ H1725 Performance Polyolefin Product Description: A specialty thermoplastic olefin compound resin with good flow, cold temperature resistance, high flexural modulus, low CLTE, and excellent paintability for automotive exterior .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI71200M High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight EPR phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM Data |
BASF Capron® BU50I Ultratough Nylon 6 (Dry)
(discontinued **) Capron Ultratough Nylon BU50I is an unfilled nylon 6 product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU5.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
BASF Ultramid® BU50I PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme .. |