Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN100TL (Dry) Nylon 66, Lubricated, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN100TL (Dry) Nylon 66, Lubricated, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: LubricatedImpact modifiedGood toughnessForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 2.30 J/cm
4.30 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
Deflection Temperature at 0.46 MPa (66 psi) 229 °C
444 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Unannealed; ASTM D648