Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celanex® 2302 GV1/15 PBT, 15% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: PBT15% glass fiber reinforced, high glossInformation provided by Celanese
Melting Point 255 °C
491 °F
ASTM D1525
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon.
Melting Point 255 °C
491 °F
DIN 53736; ASTM D789
Kolon KOPA® KN333G33BL G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Melting Point 255 °C
491 °F
DIN 53736; ASTM D789
Kolon KOPA® KN333HI2 High Impact Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Melting Point 255 °C
491 °F
Global EPP PET
PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani..
Melting Point 255 - 275 °C
491 - 527 °F
Shandong Dongyue Shenzhou New Material Co DS601 Perfluorinated Ethylene-Propylene Copolymer
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and..
Melting Point 255 °C
491 °F
Techmer ES HiFill® PA6/6 GF33 HR HS BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Hydrolysis Resistant Appearance: ..
Melting Point 255 °C
491 °F
Chase Plastics CP Pryme® NN130M2HS (Dry) Nylon 66, 30% Glass Fiber Reinforced, Lubricated, Heat Stabilized
Features: Good chemical resistanceGood compressive strengthGood creep resistanceFast cycleHeat stabilizedLubricatedHigh rigiditySolvent resistanceHigh strengthForm: PelletsInformation provided by Ch..
Melting Point 255 °C
491 °F
DSC
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren..
Melting Point 255 °C
491 °F
DSC
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac..
Melting Point 255 °C
491 °F
10°C/min,dry; ISO 11357-1/-3
DSM Akulon® Diablo HT50-HPG5 (PA66+PA6)-GF25
25% Glass Reinforced, Heat Stabilized, Blow Molding Grade
Melting Point 255 °C
491 °F
Kofler
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melting Point 255 °C
491 °F
Kofler
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melting Point 255 °C
491 °F
Kofler
CP-Polymer-Technik Wellamid® 6600 GS 30 HWCP 30% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melting Point 255 °C
491 °F
Kofler
CP-Polymer-Technik Wellamid® 6600 GV 5 HWCP 5% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melting Point 255 °C
491 °F
Kofler
CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melting Point 255 °C
491 °F
Kofler
CP-Polymer-Technik Wellamid® 6600/42 HWCP Nylon 66, Polymer Modified, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melting Point <= 255 °C
<= 491 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin
Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell..
Melting Point 255 °C
491 °F
[10 K/min], ISO 11357
Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
Melting Point 255 °C
491 °F
10°C/min; ISO 11357-1/-3
DSM Arnite® A06 700 PET (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Melting Point 255 °C
491 °F
10°C/min; ISO 11357-1/-3
DSM Arnite® AV2 372 PET-35% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Melting Point 255 °C
491 °F
10°C/min
Arkema Group Orgalloy® RS 6635 A Nylon 66 Alloy, 35% Glass Fiber (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Melting Point 255 °C
491 °F
ASTM D789
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Melting Point 255 °C
491 °F
10 K/min
BASF Ultramid® A34 01 PA66 (Dry)
Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or ..
Melting Point 255 °C
491 °F
10K/min; ISO 3146
CENTROPLAST CENTROMID 6.6 GF 30 Polyamide 6.6 30% glass fiber
This material has very high strength and rigidity, with lower moisture absorption. It can be used for housing parts, threaded bolts, and distance pieces.Information provided by CENTROPLAST Engineer..
Melting Point 255 - 275 °C
491 - 527 °F
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..
Melting Point 255 °C
491 °F
10K/min; ISO 3146
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant
This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r..
Melting Point 255 - 275 °C
491 - 527 °F
A. Schulman ComAlloy Voloy® 681 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..
Melting Point 255 - 275 °C
491 - 527 °F
A. Schulman ComAlloy Hiloy® 627 Nylon 6/6, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Melting Point 255 - 275 °C
491 - 527 °F
A. Schulman ComAlloy Hiloy® 653 Nylon 6/6, Carbon Fiber Reinforced, Flow Enhanced