Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 255 °C | 491 °F | 10°C/min; ISO 11357-1,-2,-3 |
Celanese Celanex® 2302 GV1/15 PBT, 15% Glass Reinforced
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: PBT15% glass fiber reinforced, high glossInformation provided by Celanese |
|||
Melting Point | 255 °C | 491 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnite® AV2 370 /B AV2 370 PET-35% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Melting Point | 255 °C | 491 °F | ASTM D1525 |
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66 High thermal resistant, Weather resistant, dimensionally stableApplications Cylinder head coversInformation provided by API-Kolon. |
|||
Melting Point | 255 °C | 491 °F | ASTM D1525 |
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66 G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon. |
|||
Melting Point | 255 °C | 491 °F | DIN 53736; ASTM D789 |
Kolon KOPA® KN333HB640BL Multi Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Melting Point | 255 °C | 491 °F | DIN 53736; ASTM D789 |
Kolon KOPA® KN333HI4 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Melting Point | 255 °C | 491 °F | ASTM D1525 |
Kolon KOPA® KN333HRBL Heat Resistant Nylon 66 Middle viscosity, BLACKApplications A variety of reservoir tanks and housingsInformation provided by API-Kolon. |
|||
Melting Point | 255 °C | 491 °F | |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Melting Point | 255 °C | 491 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 255 °C | 491 °F | |
Techmer ES HiFill® PA6/6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Melting Point | 255 °C | 491 °F | |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Melting Point | 255 °C | 491 °F | |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
Melting Point | 255 - 260 °C | 491 - 500 °F | |
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 255 °C | 491 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 250 GF 30 (PA6.6 + 30% glass fiber) Zellamid® 250 GF 30 (PA 6.6 + 30% Glassfibre, black) is the registered trademark for Zell-Metalls 30% glass fiber reinforced nylon grade 6.6. It offers increased strength, stiffness, creep res.. |
|||
Melting Point | 255 °C | 491 °F | DSC |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Melting Point | 255 °C | 491 °F | DSC |
Toyobo Vylopet® EMC605 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanic.. |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600 GV 30 HW 30% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWL UL-Licensed Nylon 66, Flame Protection Grade V-2, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | ASTM D2133 |
Ensinger Tecamid® MDS® Molybdenum Disulfide Filled Nylon (PA) Tecamid MDS® has enhanced surface lubricity and wear resistance over unfilled nylon. It is an ideal material to replace metals in machinery. Low surface friction Increased surface hardness Incre.. |
|||
Melting Point | 255 °C | 491 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnite® A02 307 PET Low Viscosity, Extrusion Grade |
|||
Melting Point | 255 °C | 491 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Conditioned, 40% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Lubrilon® 604 Nylon 6/6, PTFE/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Melting Point | 255 °C | 491 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Lubrilon® 635 Nylon 6/6, Carbon Fiber/PTFE Filled, Proprietary Lubricant Package Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 255 °C | 491 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnite® A02 306 PET (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |