Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic T881 Flame Retardant PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic T881 Flame Retardant PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.020 cm/cm
0.0050 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88
88
ASTM D785
Tensile Strength, Yield 58.8 MPa
8530 psi
ASTM D638
Flexural Yield Strength 88.3 MPa
12800 psi
ASTM D790
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
334 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 60 Hz
3.2

@Frequency 60 Hz
ASTM D150
Users viewing this material also viewed the following: