Cheng Yu Plastic T883GV25 Flame Retardant PBT, 25% Glass Fiber

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic T883GV25 Flame Retardant PBT, 25% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.020 cm/cm
0.0050 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Tensile Strength, Yield 111 MPa
16100 psi
ASTM D638
Flexural Yield Strength 181 MPa
26300 psi
ASTM D790
Izod Impact, Notched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 226 °C
439 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.4

@Frequency 60 Hz
3.4

@Frequency 60 Hz
ASTM D150