Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Inhibited Transformer Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Inhibited Transformer Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer components.Maximized life of oil-immersed switches — Rapid quenching of arcs reduces contact erosion.Transformer efficiency — High dielectric strength and low dissipation factor provides excellent insulating characteristics.Extended service life — Oxidation stability of Texaco Transformer Oil Inhibited limits the formation of sludges, deposits and soluble compounds which break down the electrical properties of the oil in extended service conditions.Texaco Transformer Oils are specially processed, inhibited, naphthenic transformer oils that meets ASTM D 3487 transformer oil requirements.They do not contain corrosive sulfur or harmful polychlorinated biphenyls (PCBs).The special processing and the low moisture content of Texaco Transformer Oils insure high electrical resistance, and both thermal and oxidative stability. Texaco Transformer Oils are highly stable and noncorrosive to copper.Their low pour point and low viscosity provides excellent conductive heat transfer under all operating conditions. Their high flash point offers an additional margin of safety.Texaco Transformer Oils are recommended for use in arc-forming apparatus such as:Oil-immersed transformersSwitchesCircuit breakersOil filled capacitorsTap changersElectrical reclosuresFusesThey may also be used in applications requiring low viscosity, low pour point, high quality naphthenic oils.Texaco Transformer Oils meet the requirements of:ASTM D 3487 Type I and Type II (Inhibited)British Standard BS 148 Class I and Class IA (Inhibited).Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221515; MSDS Number: 11040
Physical Properties Metric English Comments
API Gravity 28.4 °
28.4 °
Viscosity Measurement 63
63
Viscosity Index
Saybolt Viscosity at 100°F 56 SUS
56 SUS
Saybolt Viscosity at 210°F 34 SUS
34 SUS
Kinematic Viscosity at 40°C (104°F) 8.7 cSt
8.7 cSt
Kinematic Viscosity at 100°C (212°F) 2.3 cSt
2.3 cSt
Thermal Properties Metric English Comments
Pour Point -47.0 °C
-52.6 °F
Flash Point 150 °C
302 °F
Electrical Properties Metric English Comments
Dielectric Strength 50.0 kV/mm

@Thickness 1.00 mm
1270 kV/in

@Thickness 0.0394 in
ASTM D877
Descriptive Properties Value Comments
Power Factor % at 100°C 0.05