Material Notes:
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.47 g/cc
0.306 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 276 - 607 MPa
40000 - 88000 psi
Tensile Strength, Yield 103 - 172 MPa
15000 - 25000 psi
Elongation at Break 7.0 - 65 %
7.0 - 65 %
Machinability 70 %
70 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 116 W/m-K
804 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 62 - 65 %
62 - 65 %
Iron, Fe 0.15 %
0.15 %
Lead, Pb 0.80 - 1.5 %
0.80 - 1.5 %
Other, total 0.40 %
0.40 %
Zinc, Zn 32.95 - 36.65 %
32.95 - 36.65 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000663 ohm-cm
0.00000663 ohm-cm