Physical Properties Metric English Comments
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material
Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i..
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 180 Dense Refractory Castable
Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th..
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
After drying at 110°C
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable
Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values ..
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable
Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud..
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid..
Bulk Density >= 2.75 g/cc
>= 0.0994 lb/in³
Dried at 110°C
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Bulk Density >= 2.75 g/cc
>= 0.0994 lb/in³
Dried at 110°C
Sharadaa Ceramics REFCAST HA High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Bulk Density >= 2.75 g/cc
>= 0.0994 lb/in³
Dried at 110°C
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Bulk Density >= 2.75 g/cc
>= 0.0994 lb/in³
After Drying at 110°C
Sharadaa Ceramics ZAP 007 Smart Cast Application
Special Properties: Hot abrasion, Wear resistanceIndustry: SteelApplication: False Chute, Tundish BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Bulk Density >= 2.75 g/cc
>= 0.0994 lb/in³
Dried at 110°C
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Bulk Density 2.75 g/cc
0.0994 lb/in³
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation
Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par..
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
Chosun Refractories BATN-3 Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
Chosun Refractories BATN-D2, Upper Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.75 g/cc
0.0994 lb/in³
Chosun Refractories CRAG-S81 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.75 - 2.81 g/cc
0.0994 - 0.102 lb/in³
Chosun Refractories CUN-718 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density >= 2.75 g/cc
>= 0.0994 lb/in³
China-Yixing Longly Refractories Plate Corundum-Mullite
Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum..
Bulk Density 2.75 g/cc
0.0994 lb/in³
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation
Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par..