Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.014715 GPa

@Temperature 110 °C,
Time 86400 sec
2.1343 ksi

@Temperature 230 °F,
Time 24.0 hour
0.01962 GPa

@Temperature 1500 °C,
Time 10800 sec
2.846 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 58.8 MPa

@Temperature 110 °C,
Time 86400 sec
8530 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
78.5 MPa

@Temperature 1500 °C,
Time 10800 sec
11400 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage 0.00 %

@Temperature 110 °C,
Time 86400 sec
0.00 %

@Temperature 230 °F,
Time 24.0 hour
0.54 %

@Temperature 1500 °C,
Time 10800 sec
0.54 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 65 %
65 %
SiO2 27 %
27 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Main Applications Tundish
Material Required for Estimating (kg/?) 2,600
Water Required for Casting(%) 7.1