Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 1.75 g/cc
0.0632 lb/in³
Porosity 32 %
32 %
Mechanical Properties Metric English Comments
Compressive Strength 5.20 MPa

@Temperature 1350 °C,
Time 10800 sec
754 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage 0.30 %

@Temperature 1350 °C,
Time 10800 sec
0.30 %

@Temperature 2460 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 16 %
16 %
SiO2 35 %
35 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C 41
Main Applications Medium Blast Furnace
Users viewing this material also viewed the following: