Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.75 g/cc | 0.0632 lb/in³ | |
Chosun Refractories MB-2 Blast Furnace Tap-Hole Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |