Physical Properties Metric English Comments
Bulk Density 1.75 g/cc
0.0632 lb/in³
Chosun Refractories MB-2 Blast Furnace Tap-Hole Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).