Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories joint-1 Blast Furnace Runner Refractory

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories joint-1 Blast Furnace Runner Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.70 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0975 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.78 g/cc

@Temperature 110 °C,
Time 86400 sec
0.100 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0066708 GPa

@Temperature 110 °C,
Time 86400 sec
0.96753 ksi

@Temperature 230 °F,
Time 24.0 hour
0.01138 GPa

@Temperature 1500 °C,
Time 10800 sec
1.650 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 34.3 MPa

@Temperature 110 °C,
Time 86400 sec
4980 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
49.0 MPa

@Temperature 1500 °C,
Time 10800 sec
7110 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 72 %
72 %
SiO2 5.0 %
5.0 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C 17
Installation Method Block Joint
Main Applications Block joint iron runner
Water Required for Casting(%) 6.0