Material Notes:
ES-216 is available for applications where high strength and moisture resistance are required. It displays fillet formation characteristics and, after cure, is highly temperature and moisture resistant. Optimal properties are obtained with a cure cycle of two hours at 160° C.
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Shear Strength 19.3 MPa
2800 psi
Lap Shear; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C
27.8 µin/in-°F
MIL STD 883D
Thermal Conductivity 0.500 W/m-K
3.47 BTU-in/hr-ft²-°F
MIL STD 883D
Maximum Service Temperature, Air 185 °C
365 °F
Continuous
225 °C
437 °F
Intermittent
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 160 °C
2.00 hour

@Temperature 320 °F
Descriptive Properties Value Comments
Color Clear
Gross Leak Pass
Moisture Resistance Pass, 144 hrs. @ 121° C & 100% RH
Pass, 200 hrs. @ 85° C & 85% RH
Temperature Cycling Pass
MIL STD 883D
Thermal Shock Resistance (°C) Pass
MIL STD 883D