Material Notes:
Flame retardant class V0, PBDE free, high impact resistance, good melt flow rate, good light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D 955
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D 638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D 638
Elongation at Break 50 %
50 %
ASTM D 638
Flexural Modulus 2.10 GPa
305 ksi
ASTM D 790
Izod Impact, Notched 0.800 J/cm

@Temperature 0.000 °C
1.50 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C

@Load 5.00 kg
189 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
98.0 °C

@Load 0.999 kg
208 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C
1760 °F
I.E.C. 695-2-1
Users viewing this material also viewed the following: