Cotronics 454B Machinable Non-Sag Putty Adhesive

Category Polymer , Thermoset , Epoxy
Manufacturer Cotronics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics 454B Machinable Non-Sag Putty Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Viscosity 100000 cP
100000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Tensile Strength, Ultimate 68.9 MPa
10000 psi
Elongation at Break 1.2 %
1.2 %
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 5.04 W/m-K
35.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C
450 °F
Shrinkage 0.20 %
0.20 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
Dielectric Strength 17.7 kV/mm
450 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 121 °C
0.500 hour

@Temperature 250 °F