Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Covestro
Trade Name Bayflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
Bayer Test
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D638/D412
Elongation at Break 450 %
450 %
ASTM D638/D412
Flexural Modulus 0.0210 GPa
3.05 ksi
ASTM D790
Tear Strength 33.0 kN/m
188 pli
Die C; ASTM D624