Covestro Desmopan® 359 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® 359 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Desmopan 359 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
DIN 53505
Elongation at Break >= 50 %
>= 50 %
Nominal
Compression Set 30 %
30 %
70 hr; 22°C
60 %

@Temperature 70.0 °C
60 %

@Temperature 158 °F
24 hr
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 181 µm/m-°C

@Temperature 20.0 °C
101 µin/in-°F

@Temperature 68.0 °F
Copyright © lookpolymers.com All Rights Reserved