Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GS40-60 42L-NBK1 40% Glass Sphere Reinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Bead Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GS40-60 42L-NBK1 40% Glass Sphere Reinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Sphere Reinforced Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-93
Elongation at Break 10 %
10 %
ISO 527-93
Flexural Strength 110 MPa
16000 psi
ISO 178-93
Flexural Modulus 4.50 GPa
653 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-93
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0618 in
Users viewing this material also viewed the following: