Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 181 µm/m-°C @Temperature 20.0 °C |
101 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 359 Thermoplastic Polyurethane Desmopan 359 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
CTE, linear, Parallel to Flow | 181 µm/m-°C @Temperature 20.0 °C |
101 µin/in-°F @Temperature 68.0 °F |
|
Covestro Texin® 260 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |