Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Desmopan® DP 8529 Polyurethane + ABS

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyurethane Alloy , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 8529 Polyurethane + ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding grademodified with ABSgood low-temperature flexibilitygood wear resistanceApplicationSki boot shellsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
3s; ISO 868
Hardness, Shore D 60
60
15s; ISO 868
Tensile Strength at Break 64.0 MPa
9280 psi
ISO 527-1/-2
Tensile Strength, Yield 64.0 MPa
9280 psi
parallel; ISO 527-3
23.0 MPa

@Strain 100 %
3340 psi

@Strain 100 %
ISO 527-1/-2
41.0 MPa

@Strain 300 %
5950 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 30
30
mm³; ISO 4649
Compression Set 30 %

@Temperature 23.0 °C
30 %

@Temperature 73.4 °F
ISO 815
60 %

@Temperature 70.0 °C
60 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved