PreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
3s; ISO 868
Hardness, Shore D 56
56
15s; ISO 868
Tensile Strength at Break 43.0 MPa
6240 psi
ISO 527-1/-2
Tensile Strength, Yield 43.0 MPa
6240 psi
parallel; ISO 527-3
20.0 MPa

@Strain 100 %
2900 psi

@Strain 100 %
ISO 527-1/-2
43.0 MPa

@Strain 300 %
6240 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 22
22
mm³; ISO 4649
Compression Set 46 %

@Temperature 70.0 °C
46 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability North America