Material Notes:
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concentrate• High viscosity; easy release• Special grade for the coextrusion of Makrolon ET base resinsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183-1
Melt Flow 11 g/10 min

@Load 1.20 kg,
Temperature 300 °C
11 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179-1eU
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ISO 75-1,-2
Vicat Softening Point 134 °C

@Load 5.10 kg
273 °F

@Load 11.2 lb
50°C/h; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
IEC 60093
Processing Properties Metric English Comments
Melt Temperature 290 °C
554 °F
Injection molding; ISO 294
Mold Temperature 80.0 °C
176 °F
Injection molding; ISO 294
Injection Velocity 200 mm/sec
7.87 in/sec
ISO 294