Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Crucible Steel CPM® Rex® 76®(HS), AISI M48 High Speed Steel Rex® 76®(HS)

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Crucible Steel
Trade Name CPM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CPM® Rex® 76®(HS), AISI M48 High Speed Steel Rex® 76®(HS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CPM Rex 76 is a super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It is heat treatable to HRC 68-70. Its high carbon, vanadium and cobalt contents provide abrasion resistance comparable to that of T15 and red hardness superior to that of M42. With its high hardness, fine grain size and uniform carbide distribution, CPM Rex 76 is an outstanding choice for special purpose cutting tools requiring high red hardness, high abrasion resistance, and good toughness.The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 8.255 g/cc
0.2982 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 285 - 311
285 - 311
Annealed
Hardness, Rockwell C 67
67
Hardening Temperature- 1165°C; Tempering Temperature- 565°C
70
70
Hardening Temperature- 1200°C; Tempering Temperature- 525°C
Modulus of Elasticity 214 GPa
31000 ksi
Flexural Strength 2296 MPa
333000 psi
Hardening Temperature- 1200°C, Tempering Temperature- 525°C
4365 MPa
633100 psi
Hardening Temperature- 1165°C, Tempering Temperature- 565°C
Charpy Impact 8.00 J
5.90 ft-lb
Hardening Temperature- 1200°C; Tempering Temperature- 525°C
20.0 J
14.8 ft-lb
Hardening Temperature- 1165°C; Tempering Temperature- 565°C
Thermal Properties Metric English Comments
CTE, linear 10.66 µm/m-°C

@Temperature 20.0 - 95.0 °C
5.922 µin/in-°F

@Temperature 68.0 - 203 °F
10.8 µm/m-°C

@Temperature 20.0 - 200 °C
6.00 µin/in-°F

@Temperature 68.0 - 392 °F
11.74 µm/m-°C

@Temperature 20.0 - 540 °C
6.522 µin/in-°F

@Temperature 68.0 - 1000 °F
Shrinkage -0.220 %

@Treatment Temp. 1190 °C
-0.220 %

@Treatment Temp. 2170 °F
Hardening
Component Elements Properties Metric English Comments
Carbon, C 1.5 %
1.5 %
Chromium, Cr 3.75 %
3.75 %
Cobalt, Co 8.5 %
8.5 %
Iron, Fe 67.93 %
67.93 %
As Remainder
Molybdenum, Mo 5.25 %
5.25 %
Sulfur, S 0.070 - 0.22 %
0.070 - 0.22 %
Tungsten, W 9.75 %
9.75 %
Vanadium, V 3.1 %
3.1 %
Descriptive Properties Value Comments
Grindability; Metal Removed/Wheel Worn 3.8
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved