Crucible Steel SIL 1 (JIS SUH1) Martensitic Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel
Manufacturer Crucible Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel SIL 1 (JIS SUH1) Martensitic Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Crucible Specialty Metals.
Mechanical Properties Metric English Comments
Hardness, Brinell >= 269
>= 269
Hardness, Rockwell C <= 38
<= 38
Tensile Strength, Ultimate >= 932 MPa
>= 135000 psi
Tensile Strength, Yield >= 686 MPa
>= 99500 psi
Elongation at Break >= 15 %
>= 15 %
Reduction of Area >= 35 %
>= 35 %
Component Elements Properties Metric English Comments
Carbon, C 0.40 - 0.50 %
0.40 - 0.50 %
Chromium, Cr 7.5 - 9.5 %
7.5 - 9.5 %
Iron, Fe >= 85.3 %
>= 85.3 %
As Remainder
Manganese, Mn <= 0.60 %
<= 0.60 %
Nickel, Ni <= 0.60 %
<= 0.60 %
Silicon, Si 3.0 - 3.5 %
3.0 - 3.5 %
Descriptive Properties Value Comments
Heat Treatment, °C 980-1080 O.Q; 700-850 W.Q.