Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Custom Resins Norpex® 2000 PPE (Polyphenylene Ether), 20% Mineral Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Mineral Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Norpex® 2000 PPE (Polyphenylene Ether), 20% Mineral Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 74.0 MPa
10700 psi
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Izod Impact, Notched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648