Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnite® A06 300 PET (European Grade)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® A06 300 PET (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame retardant gradesEasy molding FR grades for connectorsToughened unfilled materials for durabilityHigh modulus, tight specification for critical auto componentsToughened reinforced resinsLow outgassing grades for reflector surfacesArnite extrusion resins: Specialized materials for specific usesPET for medical applicationsLoose buffer Optical fiber tubingPET for stock shapesApplicationsAutomotive:Connectors, sensors and E&E parts, Exterior fittings, Gear housings and motors, Brake valve bodiesElectrical & Electronic: Telecoms and IT connectors, Bobbins, Low voltage Power distribution, E-motor components, Lightings and Lamp fittingsConsumer Durables: Small AppliancesOther: Optical fiber tubingInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption 0.75 %
0.75 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Humidity Absorption; Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Modulus 2.50 GPa
363 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 255 °C
491 °F
10°C/min; ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Descriptive Properties Value Comments
Other Extrusion Yes
Profile extrusion Yes
Sheet extrusion Yes
Transparent Yes
Without Fillers Yes