Material Notes:
20% Glass Reinforced, Flame Retardant
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115 MPa
16700 psi
ISO 527-1/-2
Elongation at Break 2.7 %
2.7 %
ISO 527-1/-2
Tensile Modulus 8.50 GPa
1230 ksi
ISO 527-1/-2
Charpy Impact Unnotched 4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.640 J/cm²

@Temperature 23.0 °C
3.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Users viewing this material also viewed the following: