Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnitel® CM551 TPC-ES

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer DSM Engineering Plastics
Trade Name Arnitel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnitel® CM551 TPC-ES.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat Resistant Copolyester
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 51

@Time 3.00 sec
51

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ISO 527-1/-2
Elongation at Break 450 %
450 %
ISO 527-1/-2
Tensile Modulus 0.140 GPa
20.3 ksi
ISO 527-1/-2
Izod Impact Resistance NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 190 µm/m-°C
106 µin/in-°F
ISO 11359-1/-2
Melting Point 205 °C
401 °F
10°C/min; ISO 11357-1/-3
Vicat Softening Point 170 °C
338 °F
50 °C/h 50N; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.58

@Frequency 1.00e+6 Hz
3.58

@Frequency 1.00e+6 Hz
IEC 60250
4.34

@Frequency 100 Hz
4.34

@Frequency 100 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm
381 kV/in
IEC 60243-1
Dissipation Factor 0.0212

@Frequency 100 Hz
0.0212

@Frequency 100 Hz
IEC 60250
0.046

@Frequency 1.00e+6 Hz
0.046

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Users viewing this material also viewed the following: