Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DayGlo Gem-Tone GC-18F Emerald Green

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer DayGlo Color Corp.
Trade Name Gem-Tone
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DayGlo Gem-Tone GC-18F Emerald Green.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of this colorant. No blooming or plateout problems will be seen with Gem-Tone® colorants. These materials can be incorporated into polyolefin resins at levels as low as 0.05% and can be increased to higher levels to achieve the desired effect.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Bulk Density 0.513 g/cc
0.0185 lb/in³
Oil Absorption 52 %
52 %
Particle Size 20 - 80 µm
20 - 80 µm
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 288 °C
550 °F
Softening Point 77.0 - 80.0 °C
171 - 176 °F
Glass Transition Temp, Tg 70.0 °C
158 °F
Decomposition Temperature 385 °C
725 °F
Processing Properties Metric English Comments
Processing Temperature >= 177 °C
>= 350 °F
Descriptive Properties Value Comments
λmax 637nm
Abs. = 3380
718nm
Abs. = 3790