Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 70.0 °C | 158 °F | TM R050-25 |
Resinlab® EP750 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP750 Clear is a two part unfilled epoxy structural adhesive which ingredients are listed in the Code of Federal Regulations Title 21 175.105 (Adhesives) and 175.300 (Resinous and polymer.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | ISO 11359-2:1999 |
Global EPP PET PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | ISO 11359-2:1999 |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | ASTM E1640-99 (by DMA) |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Lucite International Elvacite ® 2669 Acrylic Resin Elvacite® 2669, the first in this series, is a solid acrylic bead copolymer which can be dissolved in slightly alkaline aqueous systems. This distinct capability makes the product particularly su.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond LED401 One Component LED Curable Adhesive System Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond LED401 White One Part, LED Curable Compound Description: Master Bond LED401 White is a one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond LED403Med USP Class VI, One Component, LED Curable System Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Unitika elitel UE9600 Polyester, Pellet Low viscosity type UE3600 CoatabilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, in.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond 216D02 Thixotropic No-Sag Epoxy Adhesive TRA-BOND 216D02 is a thixotropic, two part epoxy adhesive formulated specifically for applications where a nonsagging adhesive is required. TRA-BOND 216D02 works in concert with TRA-CAST 3135 to per.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond FDA2T Food and Drug Application Epoxy Adhesive TRA-BOND FDA-2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and receive.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond FS227 Thixotropic Epoxy/Polyamide Adhesive TRA-BOND FS227 is a thixotropic (thick paste) polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wettin.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Loctite® Durabond® E-30CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | ETM E-90 |
ExxonMobil ESCOREZ™ 1401 (Europe) Petroleum Hydrocarbon Resin ESCOREZ™ 1401 is a modified aliphatic hydrocarbon resin with a narrow molecular weight distribution and a high softening point. It is a tackifying resin designed to provide high temperature perform.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
DayGlo Gem-Tone GC-18F Emerald Green Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of .. |
|||
Glass Transition Temp, Tg | >= 70.0 °C | >= 158 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 320-3 Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Glass Transition Temp, Tg | >= 70.0 °C | >= 158 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | DSC 3146 |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Atom Adhesives AA-BOND FDA2T Epoxy Adhesive AA-BOND FDA2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received .. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | 10°C/min; DAM; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**) Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | TM R050-25 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Loctite® Durabond® E-60HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |