Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.2 MPa
2200 psi
Transverse to Flow; ASTM D882
17.2 MPa
2490 psi
Direction of Flow; ASTM D882
Elongation at Break 300 %
300 %
Direction of Flow; ASTM D882
500 %
500 %
Transverse to Flow; ASTM D882
Flexural Modulus 0.131 GPa
19.0 ksi
MD; ASTM D790
0.152 GPa
22.0 ksi
TD; ASTM D790
Impact 130
130
g; F50; ASTM D1709
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 35 %
35 %
45°; ASTM D2457