Diamond Polymers NPP25-1202 TF20 20% Talc Filled Copolymer Polypropylene, Impact Modified, High Heat, High Stiffness with UV and Paintable Versions

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 20% Talc Filler , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-1202 TF20 20% Talc Filled Copolymer Polypropylene, Impact Modified, High Heat, High Stiffness with UV and Paintable Versions.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ash 20 - 24 %
20 - 24 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 6.3 %
6.3 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 1.541 GPa
223.5 ksi
ASTM D790
Izod Impact, Notched 1.79 J/cm

@Thickness 3.17 mm
3.35 ft-lb/in

@Thickness 0.125 in
ASTM D256