Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP25-1602 TF40 40% Talc Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 40% Talc Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-1602 TF40 40% Talc Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Filler Content 40 %
40 %
Talc; ASTM D2584
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.3 MPa
4390 psi
chs 2.0 in/min; tangent; ASTM D638
Flexural Modulus 3.312 GPa
480.4 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 0.690 J/cm

@Temperature 23.0 °C
1.29 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648