Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 30.3 MPa | 4390 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Nanoblend™ LST 5571 Polypropylene, Unspecified (PP, Unspecified) Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demand.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM D638 |
Flint Hills AP5206-HN Polypropylene Impact Copolymer Features: Nucleated for fast cycle and good mold release. Product does not contain animal derived components.Applications: Compression and injection molding: caps and closuresInformation Provided b.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | 2 in/min (50 mm/min); ASTM D-638 |
Ineos H20A-00 Polypropylene Homopolymer A controlled rheology polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications requiring a moderate level of antistatic ag.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM Data |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 572A1V95316 Cellulose Acetate Butyrate, Smoke, Trsp Applications:Molded partsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm fee.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | chs 2.0 in/min; tangent; ASTM D638 |
Diamond Polymers NPP25-1202 TF40 40% Talc Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | chs 2.0 in/min; tangent; ASTM D638 |
Diamond Polymers NPP25-1602 TF40 40% Talc Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM Data |
Dow Retain® PS-4578 Polystyrene Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM Data |
Styron Magnum™ AG700 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | 72% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |