Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NYLON 6630 L Black

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NYLON 6630 L Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 35 - 50 %
35 - 50 %
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 1.897 GPa
275.1 ksi
ASTM D790
Izod Impact, Notched 1.59 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.98 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
ASTM D648